性能項目 | 試驗條件[狀態] | 測試方法 | 測試數據 | ||
吸水率 | 飽和(23℃) | ASTM D-570 | DAM|8.5 | % | |
吸水率 | 飽和(23℃) | ASTM D-570 | 50%RH|- | % | |
吸水率 | 24小時浸漬(23℃) | ASTM D-570 | DAM|1.2 | % | |
吸水率 | 24小時浸漬(23℃) | ASTM D-570 | 50%RH|- | % | |
比重 | ASTM D-792 | DAM|1.15 | |||
比重 | ASTM D-792 | 50%RH|1.15 | |||
荷重形變 | 13.8MPa,50℃ | ASTM D-621 | DAM|1.2 | % | |
荷重形變 | 13.8MPa,50℃ | ASTM D-621 | 50%RH|- | % | |
斷裂伸長率 | 23℃ | ASTM D-638 | DAM|30 | % | |
斷裂伸長率 | 23℃ | ASTM D-638 | 50%RH|200 | % | |
洛氏硬度R | ASTM D-785 | DAM|R121 | |||
洛氏硬度R | ASTM D-785 | 50%RH|R109 | |||
洛氏硬度M | ASTM D-785 | DAM|M87 | |||
洛氏硬度M | ASTM D-785 | 50%RH|M80 | |||
剪切強度 | 23℃ | ASTM D-732 | DAM|72.4 | MPa | |
剪切強度 | 23℃ | ASTM D-732 | 50%RH|68.9 | MPa | |
埃佐沖擊強度 | 23℃ | ASTM D-256 | DAM|43 | j/m | |
埃佐沖擊強度 | 23℃ | ASTM D-256 | 50%RH|107 | j/m | |
揉曲模量 | 23℃ | ASTM D-790 | DAM|2964 | MPa | |
揉曲模量 | 23℃ | ASTM D-790 | 50%RH|1310 | MPa | |
屈服伸長率 | ASTM D-638 | DAM|5 | % | ||
屈服伸長率 | ASTM D-638 | 50%RH|25 | % | ||
拉伸強度 | 23℃ | ASTM D-638 | DAM|90.3 | MPa | |
拉伸強度 | 23℃ | ASTM D-638 | 50%RH|62.1 | MPa | |
屈服強度 | 23℃ | DAM|90.3 | MPa | ||
屈服強度 | 23℃ | 50%RH|62.1 | MPa | ||
介電常數 | 100Hz(cps) | ASTM D-150 | DAM|4.0 | ||
介電常數 | 100Hz(cps) | ASTM D-150 | 50%RH|8.0 | ||
耗散因數 | 103Hz(cps) | ASTM D-150 | DAM|0.03 | ||
耗散因數 | 103Hz(cps) | ASTM D-150 | 50%RH|0.12 | ||
介電常數 | 103Hz(cps) | ASTM D-150 | DAM|3.9 | ||
介電常數 | 103Hz(cps) | ASTM D-150 | 50%RH|7.0 | ||
介電常數 | 106Hz(cps) | ASTM D-150 | DAM|3.6 | ||
介電常數 | 106Hz(cps) | ASTM D-150 | 50%RH|4.6 | ||
體積電阻率 | ASTM D-257 | DAM|1014 | Ω.cm | ||
體積電阻率 | ASTM D-257 | 50%RH|1012 | Ω.cm | ||
耗散因數 | 100Hz(cps) | ASTM D-150 | DAM|0.02 | ||
耗散因數 | 100Hz(cps) | ASTM D-150 | 50%RH|0.13 | ||
耗散因數 | 106Hz(cps) | ASTM D-150 | DAM|0.03 | ||
耗散因數 | 106Hz(cps) | ASTM D-150 | 50%RH|0.08 | ||
UL可燃性導級 | UL 94 | DAM|94 | |||
UL可燃性導級 | UL 94 | 50%RH|V-2 | |||
熔點 | Fisher Johns法 | ASTM D-789 | DAM|255 | ℃ | |
熔點 | Fisher Johns法 | ASTM D-789 | 50%RH|255 | ℃ | |
熱畸變溫度 | 18×106Pa | ASTM D-648 | DAM|90 | ℃ | |
熱畸變溫度 | 18×106Pa | ASTM D-648 | 50%RH|- | ℃ | |
熱畸變溫度 | (0.5)×106Pa | ASTM D-648 | DAM|240 | ℃ | |
熱畸變溫度 | (0.5)×106Pa | ASTM D-648 | 50%RH|- | ℃ | |
脆化溫度 | ASTM D-746 | DAM|-52 | ℃ | ||
脆化溫度 | ASTM D-746 | 50%RH|-52 | ℃ | ||
需氧指數 | ASTM D-2863 | DAM|25 | % | ||
需氧指數 | ASTM D-2863 | 50%RH|31 | % | ||
關于美國杜邦 BK-10A價格 | |||||
1.有關“PA66 美國杜邦 BK-10A”物性表及PA66塑料顆粒價格以出廠實時數據為準. 2.更多塑料顆粒的需求請與我們聯系. |