中等抗撞擊性 注射成型 | |
性能項目 | 試驗條件[狀態] | 測試方法 | 測試數據 | ||
比重 | ASTMD792 | 1.11 | g/cm3 | ||
熔流率(熔體流動速率)(235°C/1.0kg) | ASTMD1238 | 5.0 | g/10min | ||
收縮率-流動 | ASTMD955 | 1.5to1.9 | % | ||
抗張強度 | ASTMD638 | 65.5 | MPa | ||
伸長率(屈服) | ASTMD638 | 5.0 | % | ||
伸長率(斷裂) | ASTMD638 | 50 | % | ||
彎曲模量 | ASTMD790 | 2210 | MPa | ||
彎曲強度 | ASTMD790 | 82.7 | MPa | ||
懸壁梁缺口沖擊強度 | -40°C | ASTMD256 | 130 | J/m | |
懸壁梁缺口沖擊強度 | 23°C | ASTMD256 | 190 | J/m | |
載荷下熱變形溫度(1.8MPa,未退火) | ASTMD648 | 60.0 | °C | ||
熔融溫度 | DSC | 216 | °C | ||
線形熱膨脹系數-流動 | ASTMD696 | 8.5E-5 | cm/cm/°C | ||
RTIElec | 0.8mm | UL746 | 65.0 | °C | |
RTIElec | 1.5mm | UL746 | 65.0 | °C | |
RTIElec | 3.0mm | UL746 | 65.0 | °C | |
RTIImp | 0.8mm | UL746 | 65.0 | °C | |
RTIImp | 1.5mm | UL746 | 65.0 | °C | |
RTIImp | 3.0mm | UL746 | 65.0 | °C | |
RTIStr | 0.8mm | UL746 | 65.0 | °C | |
RTIStr | 1.5mm | UL746 | 65.0 | °C | |
RTIStr | 3.0mm | UL746 | 65.0 | °C | |
體積電阻率 | ASTMD257 | 1.0E+13 | ohmscm | ||
介電強度(3.00mm) | ASTMD149 | 12 | kV/mm | ||
相比耐漏電起痕指數(CTI) | UL746 | 600 | V | ||
UL阻燃等級(0.8mm) | UL94 | HB | |||
極限氧指數 | ASTMD2863 | 21 | % | ||
關于Chem Polymer公司 Chemlon® 253價格 | |||||
1.有關“PA6 Chem Polymer公司 Chemlon® 253”物性表及PA6塑料顆粒價格以出廠實時數據為準. 2.更多塑料原料的需求請與我們聯系,電話同微信:186-2131-7168 |
本文鏈接:http://www.tebozhan.com/showinfo-41-21328-0.htmlPA6 Chem Polymer公司 Chemlon® 253
聲明:本網頁內容旨在傳播知識,若有侵權等問題請及時與本網聯系,我們將在第一時間刪除處理。郵件:2376512515@qq.com